| PTN501 | 耐燃气炉黄变,在250°C烘烤条件下,具有较好的抗黄变性能 Resistant to yellowing in gas furnaces, and has good anti-yellowing performance under 250°C baking conditions | 0.3-1%(预混) pre-blending |
| PTN502 | 耐燃气炉和高温黄变,浅白色粉末在250°C烘烤条件下色差较小 Resistant to yellowing in gas furnaces and high temperatures, the light white powder has little color difference when baked at 250°C | 0.3-1%(预混) pre-blending |
| PTN503 | 显著抑制浅白色粉末因为燃气炉和高温烘烤产生的黄变现象 Significantly inhibits the yellowing of light white powder caused by gas furnace and high temperature baking | 0.3-1%(预混) pre-blending |
| PTN504 | 耐燃气炉和高温黄变,浅白色粉末在300°C烘烤条件下色差较小 Resistant to yellowing in gas furnaces and high temperatures, the light white powder has little color difference when baked at 300°C | 0.3-1%(预混) pre-blending |
| PTN505 | HAA体系专用抗黄变剂,有效改善涂层耐燃气炉和高温烘烤产生的黄变现象 Special anti-yellowing agent for HAA system, effectively improving the yellowing phenomenon caused by the coating's resistance to gas and high-temperature baking | 0.5-1.5%(预混) pre-blending |
| PTN506 | 用于300/600度高温粉末涂料,提升涂层在高温烘烤下的稳定性 Used for 300/600 degree high temperature powder coating to improve the stability of the coating under high temperature baking | 2-5%(预混) pre-blending |
| PTN507 | 用于500/700度高温粉末涂料,提升涂层在高温烘烤下的稳定性 Used for 500/700 degree high temperature powder coating to improve the stability of the coating under high temperature baking | 2-5%(预混) pre-blending |
| PTN508 | 用于500/700度高温粉末涂料,提升涂层在高温烘烤下的稳定性 Used for 500/700 degree high temperature powder coating to improve the stability of the coating under high temperature baking | 2-5%(预混) pre-blending |